Proses Anil & Perlakuan Panas
Proses anil merupakan proses perlakuan panas suatu bahan melalui pemanasan pada temperatur cukup tinggi dan waktu yang lama, diikuti pendinginan perlahan-lahan
Anil
Tujuan: menghilangkan tegangan sisa & menghindari terjadinya retakan panas
Prosedur: temperatur pemanasan mendekati temperatur transisi gelas dan
pendinginan perlahan-lahan
Perubahan strukturmikro: tidak ada
Anil sempurna
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEjels9kJiUPg5W1JQ-Up8ruerYslJYGZv5rLPBi3gfAvOzhkjvix_F7eKmeMkGShy4j-KfRt9l2bq7XXzQbDufi6prZ6ZfDWgEJ34aGU1NkuQBz4J0zEZkgWW26QoWZqd5_Nt7tGIDckpPS/s400/ANIL.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEhGf__uLHj4kS0MJ8ppa9-250urjdpOasrjUxQnqaKCEd7vOmL857AAlbs0YjLmK6ouy2MtPDIIjUK4k6VKRqtK24yWS4wMc3g-LmLMNV11t1mtmx8Z92N4enWBR2o5YM86imYhYXp-t2OZ/s400/aa.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEj8nX1H4fIL0svfD5xpqXGCuN8tl1khF5MQ8dpbtaCo8nJV4EHL5PqHegoT0J_DTyBOg1UmhCXZNsHzMWrDDuswwDInOwqyXErpLZFJJ9z6pKFn3Zs8qu1HaZLVoZdqF5vLqpIm43EFdt87/s400/1a.png)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEgAJGTMozicufZCg_f2ZHCwZsPpJM0eoZ39qihuTpzFt77SXzptmrtib2ECsGsQUgPF9xiexLyQziU8DY4bbp19Som3hVZw1u5Eoq-wDxX9Oz3BeoLJ7BJRvcSJ9UJF8K9tbbkSxJo6Ws3f/s400/1b.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEhoaBD51uRhnROrFWMNWKW8tn1fvkxuiFY5YzWCGJAwES13JM48nSDI_KD20p_MFKch9oeHC-CA-ocilDSBEOc_pkWLh6lOXJgr3ZSKoEVPBhTQhe_p-GdlGe-AnBGGOE0paeWBCfyPtsLK/s400/1c.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEhvSMmLjC6PmXFAFfTUdSdNm_DNE-kF2RQHPMkuNnw9yt4cs58tF-vf-tjBujPiadHJoOBn2dHMFYQD76Qe3YBW3QIVv-b0C_dP6jwgm8rJWNFw6J9DH1p4qL7IMQI7Q7k67Be8tKgd9ZfM/s400/1d.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEgo40Lsx7HRPaXG7xnNuH6f4KOswpaupyNMED0vLFi9U4Tc3_4H1kS2K4cQAAUKWWJAngzvXQNgTUGWQ-SXT443XqFQ67KHPdf3JuipRkOE9htr0SWXs7JF_DKH4tLQuADX7d-vPRkH3fhy/s400/1e.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEi_wx98ad-mmAzb_hDK30jZ8WMrPkJVSrg28W2dkYEz3cwNBnkgUr5Y9m_95Tz8V_0vZES0kQaNlxobhvHbL7DaZeFvBcaZF3wJMMNIEB-9oOevsX8dqyxlWpH6rAA8ppvC6XwrPKjm3cEh/s400/1f.jpg)
![](https://blogger.googleusercontent.com/img/b/R29vZ2xl/AVvXsEihcTapySqN538FfIP6QnMdKZXhSSw1pmya8c1CiUVopZ3_MyWp1Qrz4jfq9OIZmjvKSC9lplzdohZQ9yllZ1GRsVnZXbEzhdnHPItliBsE5SKYcv-rCyhNEeuSJfUaau1Y4Rr3KWPob-mG/s400/1g.jpg)
Tidak ada komentar:
Posting Komentar